PrimaSelect NylonPower Glass Fibre - 1.75mm - 500g - Natural
Most items delivered in 1-2 working days.
Contact us here or
call us on +44 1530 811 004
Most items delivered in 1-2 working days.
Contact us here or
call us on +44 1530 811 004
PrimaSelect NylonPower Glass Fiber is the latest high-performance filament for your 3D printer. The material is based on Nylon 12 and is 16 % glass fiber reinforced. This composition results in an optimally resistant filament. Nylon glass filament is perfect for additive manufacturing of components for the automotive industry, drone construction and RC parts.
PrimaSelect NylonPower Glass Fiber is an extremely useful material with very unique material properties. In this filament, the nylon is reinforced with small, cut glass fiber strands. PrimaSelect NylonPower Filament offers you incredible stiffness, structure and excellent layer adhesion.
Furthermore NylonPower is very easy to process and has a matt surface. The perfect 3D prints are very stiff, rigid and ideal if you need an object with a high stiffness/weight ratio. To process PrimaSelect NylonPower Filament, use a heated printing bed - set to 60 ˚C - to achieve good adhesion of the first layer to the building platform.
Because of the highly abrasive properties of PrimaSelect NylonPower (the nozzle wears quickly due to abrasion), we recommend that you use a hardened steel nozzle for this filament. Using a normal brass nozzle is not a problem, but the nozzle will wear out in a short time.
PrimaSelect NylonPower adheres to glass coated with adhesive spray or adhesive.
Here you’ll find tips and tricks for processing PrimaSelect NylonPower with glass fibers on your 3D printer.
The glass fibers contained in PrimaSelect NylonPower reduce the amount of water that can be absorbed. However, for optimal processing you should take care to keep the filament away from moisture and to protect it.
To do this, you must store PrimaCreator NylonPower in a dry place immediately after unpacking. The filament is supplied in a vacuum-sealed bag with desiccant so that the first 3D print succeeds immediately and gives you a perfect result.
In case of exposure to moisture, we strongly recommend that you dry your NylonPower glass fibre filament before starting 3D printing. To do this, simply place the entire coil in the oven at 80 °C for 5 to 7 hours. This will dry your coil and allow you to start a new 3D print.
PrimaSelect NylonPower requires an extruder temperature of 250 - 265 °C for optimal extrusion. This filament can be processed on most 3D printers. However, we strongly recommend that you use a full metal extruder for higher temperatures. PrimaSelect NylonPower glass fibre filament can be processed at lower temperatures, too. However, you should always keep in mind that you will not get the same strength in the finished parts when using lower temperatures.
This filament contains glass fibers, making it very abrasive for your nozzle. We strongly recommend that you use a hardened steel nozzle for this filament, as a normal brass nozzle will be worn out by nylon filament in a very short time.
Larger 0.6 or 0.8 mm nozzles produce very strong 3D prints and reduce the risk of clogging the nozzle. However, you can also use it with a 0.4 mm nozzle.
NylonPower glass fibre does not adhere well to PEI, BuildTak, or similar surfaces. Glass is the best surface for use with Magigoo, PrintaFix, PVA-based glue stick or further adhesives. Do not use fans when 3D printing with NylonPower.
Buy PrimaSelect NylonPower Glass Fiber and you'll get the latest generation of high-performance filament for your 3D printer.
Basic Data | |
Filament Typ | NylonPower Glass Fibre |
Diameter | 1,75 mm |
Tolerance | 0,05 mm |
Weight | 0,50 kg |
Lenght | 194 m |
Color | - ohne Color Code |
Printing Parameter | |
Recomended Printing Temp Min | 250 ºC |
Recomended Printing Temp Max | 265 ºC |
Recomended Printbed Temperature Min | 60 ºC |
Recomended Printbed Temperature Max | 70 ºC |
Recomended Printing Speed Min | 40 mm/s |
Recommended Printing Speed Max | 40 mm/s |
Recomended Fan Speed Min | 20 % |
Recomended Fan Speed Max | 60 % |
General | |
Specific gravity | 1,07 g/cm3 ISO 1183 |
Mold Shrinkage | ,5 ISO 294 |
Specific volume resistivity | 10^11 Ωm IEC 60243 |
Temperature | |
Heat deflection temp | 160 °C ISO 75 |
Tensile | |
Tensile strength | 64,7 MPa ISO 527 |
Tensile modulus | 2534 MPa ISO 527 |
Elongation | |
Elongation at break | 9,2 % ISO 527 |
Flexural | |
Flexural Strenght | 125 % ISO 178 |
Flexural Modulus | 3131 ISO 178 |
Other | |
Impact Strength | 53,6 KJ/m2 ISO 179ISO 1802-1eU |
Shore D Hardness | 77 MPa D ISO 2039-1 |